CHARACTERISTICS OF PLASTIC BONDED MAGNETS
- one molding and can achieve precision dimensional accuracy;
- easy to be processed directly into thin-walled ring, tile and other shapes;
- can be magnetized, multi-polar magnetization;
- it is more resistant to corrosion than sintered magnets;
- An anisotropic bonded magnets with higher magnetic properties can be developed.
- easy to be processed directly into thin-walled ring, tile and other shapes;
- can be magnetized, multi-polar magnetization;
- it is more resistant to corrosion than sintered magnets;
- An anisotropic bonded magnets with higher magnetic properties can be developed.
MATERIAL CHARACTERISTICS
Grade |
Residual Induction Br |
Coercive Force Hcb |
Intrinsic Coercive Force Hcj |
Max. Energy Product (BH)max. |
Material |
Application |
JPM-N4 |
530~630mT |
200~340kA/m |
450~665kA/m |
28~49.6kJ/m3 |
Nd2Fe14B |
Holder Stationery Toy Household Appliance OA Facilities Micro-motor |
5300~6300Gs |
2513~4272Oe |
5655~8356Oe |
3.5~6.2MGOe |
|||
JPM-N6 |
600~700mT |
360~440kA/m |
600~800kA/m |
49.6~64kJ/m3 |
Nd2Fe14B |
|
6000~7000Gs |
4524~5529Oe |
7540~10053Oe |
6.2~8.0MGOe |
|||
JPM-N8 |
600~700mT |
400~480kA/m |
640~800kA/m |
64~76kJ/m3 |
Nd2Fe14B |
|
6000~7000Gs |
5026~6031Oe |
8042~10053Oe |
8.0~9.5MGOe |
|||
JPM-N8L |
600~700mT |
320~448kA/m |
560~720kA/m |
60~72kJ/m3 |
Nd2Fe14B |
|
6000~7000Gs |
4021~5629Oe |
7037~9047Oe |
7.5~9.0MGOe |
|||
JPM-N8H |
560~650mT |
400~480kA/m |
875~1200kA/m |
60~76kJ/m3 |
Nd2Fe14B |
|
5600~6500Gs |
5026~6031Oe |
10995~15079Oe |
7.5~9.5MGOe |
|||
JPM-N10 |
650~750mT |
400~480kA/m |
680~850kA/m |
72~88kJ/m3 |
Nd2Fe14B |
|
6500~7500Gs |
5026~6031Oe |
8545~10681Oe |
9.0~11.0MGOe |
|||
JPM-N10L |
700~800mT |
400~480kA/m |
480~640kA/m |
72~88kJ/m3 |
Nd2Fe14B |
|
7000~8000Gs |
5026~6031Oe |
6031~8042Oe |
9.0~11.0MGOe |
|||
JPM-N10H |
650~750mT |
430~510kA/m |
875~1035kA/m |
72~88kJ/m3 |
Nd2Fe14B |
|
6500~7500Gs |
5403~6408Oe |
10995~13000Oe |
9.0~11.0MGOe |
|||
JPM-N12 |
700~770mT |
450~530kA/m |
680~850kA/m |
80~96kJ/m3 |
Nd2Fe14B |
|
7000~7700Gs |
5655~6660Oe |
8545~10681Oe |
10.0~12.0MGOe |
|||
JPM-N12L |
750-830mT |
380-460kA/m |
480~640kA/m |
80-96kJ/m3 |
Nd2Fe14B |
|
7500-8300Gs |
4773-5777Oe |
6031~8042Oe |
10.0-12.0MGOe |
|||
JPM-N12H |
740-790mT |
460-540kA/m |
716~836kA/m |
80-100kJ/m3 |
Nd2Fe14B |
|
7400-7900Gs |
5780-6785Oe |
9000~10500Oe |
11.0-12.5MGOe |
Other Physical Characteristics
Grade |
Density g/cm3 |
Hardness HRB |
Temperature Coefficient %/℃ |
Curie Temperature ℃ |
Max Operation Temperature ℃ |
Saturated Magnetic Field kA/m |
Thickness Of Coating μm |
JPM-N4 |
5.8~6.3 |
40~45 |
-0.11 |
≥350 |
120-160 |
≥1600 |
5~30 |
JPM-N6 |
5.8~6.1 |
40~45 |
-0.11 |
≥350 |
120-160 |
≥1600 |
5~30 |
JPM-N8 |
5.8~6.1 |
35~38 |
-0.11 |
≥350 |
120-160 |
≥1600 |
5~30 |
JPM-N8L |
5.8~6.1 |
35~38 |
-0.12 |
≥400 |
110-140 |
≥1600 |
5~30 |
JPM-N8H |
5.8~6.1 |
35~38 |
-0.12 |
≥300 |
150-170 |
≥2400 |
5~30 |
JPM-N10 |
5.8~6.1 |
35~38 |
-0.10 |
≥350 |
120-160 |
≥1600 |
5~30 |
JPM-N10L |
5.8~6.1 |
35~38 |
-0.10 |
≥320 |
110-150 |
≥1600 |
5~30 |
JPM-N10H |
5.9~6.2 |
35~38 |
-0.10 |
≥400 |
150-180 |
≥2000 |
5~30 |
JPM-N12 |
6.0~6.3 |
35~38 |
-0.10 |
≥350 |
120-160 |
≥1600 |
5~30 |
JPM-N12L |
6.0~6.3 |
35~38 |
-0.10 |
≥320 |
110-150 |
≥1600 |
5~30 |
JPM-N12H |
6.0~6.3 |
35~38 |
-0.11 |
≥350 |
120-160 |
≥1600 |
5~30 |
*The coating material can be chosen according to customer,s demand
PRODUCT ADVANTAGE
QUALITY
PRODUCTION PROCESS FLOWCHART
MAGNETIZATION DIRECTION
-
Axial
-
Diametrical
-
Axial
-
Diametrical
-
Thickness
-
Length
-
Axial
-
Diametrical
-
Diametrical
-
Diametrical
-
Width
-
Thickness